A516 Grade 70 Mill Test Certificate Explained

A516 Grade 70 mill test certificate
Picture of Chiranjiv Steel Centre

Chiranjiv Steel Centre

Share this read
Table of contents
Pressure vessel plates
Need A516 Grade 70 plates with full certification?
1 min
Use AI to summarize this article

A mill test certificate is the document that proves a plate is what the purchase order asked for. It records the heat of steel the plate came from, the chemical analysis of that heat, the mechanical test results, the delivery condition and any additional testing that was carried out. Without it, a plate is just steel of unknown origin.

For A516 Grade 70 the certificate carries more weight than it does for structural plate. Pressure vessel work depends on controlled steelmaking, verified properties and an unbroken traceability chain, and the certificate is where all three are evidenced. On a code-stamped vessel it is also what an Authorized Inspector examines before accepting the material.

This blog explains each part of an A516 Grade 70 mill test certificate: what the EN 10204 certificate types mean, what values to check for Grade 70, why some fields are blank, and the mistakes people often find during inspection. 

What a Mill Test Certificate is

A mill test certificate, commonly shortened to MTC, is issued by the steel mill and certifies that the material supplied meets the requirements of the specification named on it. You will also see it called a material test certificate or, in North American usage, a mill test report or MTR. The three terms describe the same document.

Its purpose is twofold. It records what the material is, through chemical and mechanical test results, and it records where the material came from, through the heat number that ties the plate back to a specific melt at the mill.

That second function is easy to underestimate. If a problem emerges years later, the heat number is what allows every plate from that melt to be identified and reviewed.

EN 10204 Certificate Types

EN 10204 defines four types of inspection document. The difference between them is who performed the inspection and whose results appear on the certificate.

Type Name What it provides
2.1 Declaration of compliance with the order The manufacturer states the product complies. No test results at all.
2.2 Test report The manufacturer states compliance and supplies results from non-specific inspection, meaning results not taken from your material.
3.1 Inspection certificate 3.1 Results from specific inspection on the actual product supplied, validated by the manufacturer’s authorised inspection representative, independent of the manufacturing department.
3.2 Inspection certificate 3.2 As 3.1, but additionally validated by the purchaser’s representative or an independent third party inspector.

Type 3.1 is the normal minimum for A516 Grade 70. It is the standard across oil and gas, petrochemical and power projects because the results relate to the plate you actually received.

Type 3.2 is specified for critical work where independent verification is required, such as subsea, nuclear or high-pressure duty, or wherever a client mandates third party inspection by an organisation such as Bureau Veritas, SGS, TÜV or Lloyd’s Register. A Type 3.2 certificate carries two sets of signatures and stamps.

Types 2.1 and 2.2 should not be accepted for pressure vessel plate. A 2.2 certificate may look reassuring because it contains numbers, but those numbers may come from different material entirely.

One point worth checking on receipt: a Type 3.1 certificate does not satisfy an order that specified 3.2. Substituting downward is a legitimate ground for rejection.

Heat Number and Traceability

Heat number hard stamped on an A516 Grade 70 steel plate

The heat number, sometimes called the cast number, identifies the batch of molten steel the plate was rolled from. Every certificate carries it, and it is the anchor of the entire traceability chain.

Two checks matter here.

The heat number on the certificate must match the marking on the plate. A516 Grade 70 is normally hard stamped, paint stencilled, or both. If the physical marking and the paperwork disagree, stop and resolve it before the plate is cut, because once a plate is cut into parts the identification can be lost.

Plate numbers should also correlate. Many mills issue a plate or piece number alongside the heat number, allowing an individual plate to be traced rather than just the melt it came from.

If your fabrication involves cutting plates into smaller pieces, transferring the heat number onto each piece before cutting is standard practice, and on code work it is a requirement.

Grade and Specification: A516 or SA516

The certificate must name the specification and grade, and this field deserves closer attention than it usually gets.

For a code-stamped vessel built to the ASME Boiler and Pressure Vessel Code, the certificate must name SA-516 Grade 70. A certificate naming only ASTM A516 Grade 70 will not satisfy an Authorized Inspector, even though the steel and the test results are identical. Most mills avoid the problem by dual certifying to both, and both designations then appear on the certificate.

This trips up more orders than any other single field, and it is worth understanding the reasoning behind it rather than treating it as a formality. The difference between ASTM A516 and ASME SA516 is entirely a matter of which body publishes the standard and what the material may be used for.

Also confirm the suffix. Where normalized plate was ordered, the certificate should show Grade 70N or state the normalized condition explicitly.

Chemical Composition: Heat Analysis and Product Analysis

Laboratory chemical analysis of a steel plate sample

The certificate lists actual measured percentages for each element, which you compare against the specification limits. For A516 Grade 70 the elements reported are carbon, manganese, phosphorus, sulphur and silicon, and most mills add others they have measured.

What causes unnecessary rejections is the difference between the two types of analysis.

Heat analysis, also called ladle or cast analysis, is taken from the molten steel during casting. This is what the mill controls to, and it is what appears on most certificates.

Product analysis is taken from the finished plate. Because elements segregate slightly as steel solidifies, a product reading can drift outside the heat analysis range without the plate being non-conforming. The specification allows a wider tolerance for exactly this reason.

The practical effect on Grade 70 is that manganese has a heat analysis range of 0.85 to 1.20% but a product analysis range of 0.79 to 1.30%. Silicon behaves the same way, at 0.15 to 0.40% on heat analysis and 0.13 to 0.45% on product analysis. So a manganese reading of 1.26% on a product analysis is within specification even though it sits above the heat analysis ceiling.

Before querying a chemistry result, check which analysis the certificate is reporting.

Product analysis is not carried out as standard. It is Supplementary Requirement S2 under ASTM A20, and appears only if the purchase order asked for it.

Mechanical Test Results

Tensile testing machine measuring steel plate strength

This section reports the tensile test carried out on a coupon taken from the plate. Three values matter, and each has its own acceptance rule.

Property Requirement What to watch
Tensile strength 485–620 MPa (70–90 ksi) Both limits apply
Yield strength 260 MPa (38 ksi) minimum No upper limit
Elongation 17% in 200 mm or 21% in 50 mm Check which gauge was used

Tensile strength has a ceiling as well as a floor. This is the check most often missed. A result of 640 MPa fails the specification just as surely as one of 470 MPa, because A516 is a toughness-first specification and steel that is too strong is usually too brittle. Plate testing above 620 MPa is rejectable.

Yield strength has a minimum only. A result of 340 MPa is perfectly acceptable and common.

Elongation depends on the gauge length used. The mill reports whichever it used, and you need to compare against the matching figure. Comparing an 8 inch result against the 2 inch requirement will produce a false rejection.

Tensile specimens for A516 plate are normally taken transverse to the rolling direction under ASTM A20, and the certificate will usually state the orientation.

For a fuller explanation of where these figures come from and how thickness affects them, see the mechanical properties of A516 Grade 70 plate.

There is one further allowance worth knowing before rejecting a low elongation result. ASTM A20 permits deductions from the minimum elongation on very thin plate below roughly 8 mm and on very thick plate above 89 mm. A result slightly under 17% on a 150 mm plate may still conform, so check the thickness first.

Delivery Condition and Heat Treatment

Steel plate entering a normalizing furnace for heat treatment

The certificate records the condition the plate was supplied in. For A516 Grade 70 you will see one of the following:

  • As-rolled, meaning no heat treatment after rolling
  • Normalized, meaning reheated to roughly 900 °C and cooled in still air
  • Normalized and stress relieved, where a subsequent stress relief cycle was applied

The rule to check against is thickness. Plate over 40 mm is normalized as standard. Plate up to 40 mm is supplied as-rolled unless normalizing was specified on the order.

This is a genuine rejection point. If you ordered normalized plate for cold service and the certificate says as-rolled, the material does not meet your order regardless of how good the tensile results look. Where normalizing is certified, the certificate should confirm the temperature and that the plate was air cooled.

Supplementary Test Results

A516 Grade 70 has a small set of mandatory tests. Everything beyond that is a supplementary requirement under ASTM A20, invoked by number on the purchase order, and it appears on the certificate only if it was ordered.

Test Requirement Typically reported as
Charpy V-notch impact S5 Three individual values plus average, at a stated temperature
Product chemical analysis S2 A second chemistry row
Simulated post-weld heat treatment S3 Test coupons cycled before testing
Ultrasonic examination S8, S11 or S12 Pass or fail against the stated acceptance standard

The important point for incoming inspection is that a blank field is not a defect if you did not order the test. Certificates are frequently queried because no impact values appear, when impact testing was never specified.

Where impact testing was ordered, check three things: the test temperature matches your requirement, the absorbed energy meets the specified minimum, and the specimen orientation is what you asked for. A common process industry requirement for Grade 70 is 27 J average at −46 °C on normalized plate.

Sour service orders add further tests, typically HIC testing to NACE TM0284 and a hardness cap for NACE MR0175 compliance. Both appear on the certificate only when specified.

Carbon Equivalent

Many mills report a carbon equivalent value even though A516 does not require one. For Grade 70 it typically falls between 0.43 and 0.45.

This figure is for your welding engineer rather than your inspector. It indicates how susceptible the heat-affected zone will be to hydrogen cracking, and it feeds directly into the preheat temperature set in the welding procedure. On thicker plate, where carbon content is permitted to rise, the value tends to climb with it.

If the certificate does not report it, the welding engineer can calculate it from the chemistry that is reported.

How to Verify an A516 Grade 70 Certificate

Inspector checking mill test certificates against steel plate stock

Work through the certificate in this order during incoming inspection.

  1. Certificate type. Does the EN 10204 type match the purchase order? A 3.1 will not satisfy an order specifying 3.2.
  2. Specification and grade. Is SA-516 named if the vessel is code stamped? Is the grade correct?
  3. Heat number. Does it match the marking on the physical plate?
  4. Dimensions. Do thickness, width and length match what was ordered?
  5. Chemistry. Are all elements within limits, and is the correct analysis type being compared?
  6. Tensile and yield. Is tensile inside 485 to 620 MPa, and yield at or above 260 MPa?
  7. Elongation. Which gauge length, and does it meet the matching requirement after any A20 thickness allowance?
  8. Delivery condition. As-rolled or normalized, and does it match the order?
  9. Supplementary results. Are all ordered tests present and passing?
  10. Signatures and stamps. Is the certificate signed by the mill’s authorised representative, and by the third party inspector where 3.2 was specified?

Anything that fails should be raised before the plate is cut. After cutting, the commercial position weakens considerably.

Common Errors Found on Mill Test Certificates

These surface regularly during incoming inspection.

  • Only A516 named where SA-516 was required. The most frequent cause of rejected paperwork on code projects.
  • Delivery condition does not match the order. As-rolled supplied where normalized was specified.
  • Wrong certificate type. Type 3.1 issued against an order specifying 3.2.
  • Heat number mismatch between the certificate and the plate marking.
  • Missing supplementary results where impact or ultrasonic testing was ordered.
  • Impact testing at the wrong temperature, for example −20 °C where −46 °C was required.
  • Transposed or incomplete dimensions, which matters where plates are being allocated to specific components.

Note which of these are certificate problems and which are material problems. A missing designation can often be corrected by the mill reissuing the document. A plate normalized when it should not have been, or not normalized when it should have been, cannot be fixed by paperwork.

Checking a Certificate Is Genuine

Falsified certificates exist, particularly on material bought through unfamiliar trading chains rather than direct from a mill or established stockholder.

Practical checks:

  • Contact the mill directly with the heat number and certificate number. Most major mills will confirm whether a certificate they issued exists.
  • Look at internal consistency. Do the chemistry values plausibly produce the reported mechanical results? A very low carbon and manganese combination reporting high tensile strength does not add up.
  • Check the mill actually produces the product. A certificate from a mill that does not roll heavy plate is a warning sign.
  • Examine the document itself. Mismatched fonts, misaligned tables and altered-looking figures are worth questioning.
  • Verify signatures and stamps are present, and that a Type 3.2 carries both required validations.

Where material is critical and the supply chain is unfamiliar, third party inspection at the mill is the reliable answer rather than document checking after delivery.

The role of a Mill Test Certificate Explained properly in the buying process is preventive. It is far cheaper to resolve a documentation problem at enquiry stage than at incoming inspection.

Frequently Asked Questions

What is a mill test certificate?

It is a document issued by the steel mill certifying that the material supplied meets the requirements of the specification named on it. It records the heat number, chemical analysis, mechanical test results, delivery condition and any supplementary testing carried out. For pressure vessel plate it is also the basis of traceability back to the original melt.

Is an MTR the same as an MTC?

Yes. Mill test report and mill test certificate describe the same document, with MTR more common in North American usage. Material test certificate is a third name for it. All three should contain the same information.

What is the difference between EN 10204 3.1 and 3.2?

Both report results from specific inspection on the actual material supplied. A Type 3.1 is validated by the manufacturer’s authorised inspection representative, who must be independent of the manufacturing department. A Type 3.2 adds validation by the purchaser’s representative or an independent third party inspector, so it carries two sets of signatures and stamps.

What should an A516 Grade 70 mill test certificate show?

At minimum the heat number, specification and grade, plate dimensions, chemical analysis, tensile and yield strength, elongation, and the delivery condition. Where supplementary requirements were ordered, it should also show those results, most commonly Charpy impact values and ultrasonic examination. For code work it must name SA-516.

Can I reject a plate if the tensile strength is too high?

Yes. A516 Grade 70 specifies a tensile range of 485 to 620 MPa, so a result above 620 MPa is non-conforming. This surprises buyers who assume stronger is always acceptable, but excessive strength usually indicates reduced toughness, which is the property A516 exists to guarantee.

Why does the certificate show manganese above the specified range?

Almost certainly because it is reporting a product analysis rather than a heat analysis. Product analysis is taken from the finished plate, where slight segregation during solidification shifts the readings, so the specification permits a wider tolerance. For manganese the heat analysis range is 0.85 to 1.20% while product analysis allows 0.79 to 1.30%.

What is a heat number and why does it matter?

It identifies the specific batch of molten steel the plate was rolled from. It is the link between the physical plate and every test result on the certificate, and it allows material to be traced years later if a problem emerges. It should be verified against the marking on the plate itself on receipt.

Do I need a 3.2 certificate for A516 Grade 70?

Not usually. Type 3.1 is the standard requirement for most pressure vessel work. Type 3.2 is specified where independent verification is required by the client or the design code, typically on critical service such as subsea, nuclear or high-pressure duty. Ordering 3.2 unnecessarily adds cost and lead time.

Why are there no impact test results on my certificate?

Because Charpy V-notch testing is a supplementary requirement rather than a standard one. Unless the purchase order invoked it, the mill did not perform it and the certificate will not report it. This is not a defect in the certificate, though it does mean the plate cannot be used where impact values are required.

Final Checks

An A516 Grade 70 mill test certificate is worth reading properly rather than filing on arrival. The fields that most often cause problems are the specification designation, the delivery condition and the certificate type, and all three are far easier to resolve before the plate is cut.

Three habits prevent most disputes. Specify everything you need at enquiry stage, including certificate type, delivery condition and any supplementary testing. Check the heat number against the plate marking on receipt. And compare each result against the correct limit, remembering that tensile strength has a ceiling, elongation depends on the gauge length, and a blank field for a test you never ordered is not a defect.