ASTM A516 Grade 70 is a carbon steel plate built for welded pressure vessels running at moderate and lower temperatures. It is the strongest of the four A516 grades and the most widely stocked worldwide. You may also see it written as SA516 Grade 70, which is the same steel adopted into the ASME Boiler and Pressure Vessel Code.

Mechanical properties describe the way the plate behaves under load, and four of them do most of the work. Tensile strength is the maximum stress the plate carries before it begins to break. Yield strength is the point where it stops springing back and starts to deform permanently. Elongation measures the stretch before fracture, which tells you the ductility. Impact toughness shows whether the plate absorbs a sudden blow or cracks instead, and it matters most in cold service. For Grade 70, the required figures are 485–620 MPa tensile strength, a minimum yield of 260 MPa, and at least 17% elongation.

Below, each property is covered in detail, along with hardness and the impact testing rules. We also look at the effect of plate thickness and heat treatment, the translation into allowable stress under ASME, a comparison against other grades and equivalents, and the checks worth making on your mill test certificate.

A516 Grade 70 Mechanical Properties: Full Table

These are the values the standard requires. They will be confirmed on your Mill Test Certificate (MTC).

Property Metric Imperial
Tensile strength 485–620 MPa 70–90 ksi
Yield strength (minimum) 260 MPa 38 ksi
Elongation in 200 mm (min) 17% 17% in 8 in.
Elongation in 50 mm (min) 21% 21% in 2 in.
Hardness (typical, not specified) 130–200 HB 130–200 HB
Charpy V-notch impact Supplementary requirement only Supplementary requirement only

Two details are easy to miss:

Tensile strength is a range, not a minimum. Yield strength has only a floor of 260 MPa. Tensile strength has a floor and a ceiling. Material testing above 620 MPa fails the specification just as surely as material testing below 485 MPa.

Tensile tests are taken across the rolling direction. Under ASTM A20, tensile specimens for A516 plate are normally prepared in the transverse direction. Steel is slightly stronger and more ductile along the rolling direction, so transverse testing gives the more conservative measurement.

Tensile Strength of A516 Grade 70

Tensile strength is the maximum stress the plate can carry before it starts to break. For Grade 70 this is 485–620 MPa (70–90 ksi).

Why does the standard put a maximum on it? Because a pressure vessel is designed to deform before it fails. Steel that is too strong is usually also too hard and too brittle, which makes it harder to form into shells and heads, harder to weld without cracking, and less forgiving of an overload. A516 is a toughness-first specification, so it caps the strength deliberately.

In practice, mill-supplied Grade 70 plate usually tests somewhere in the 510–570 MPa band, comfortably inside the window.

Yield Strength of A516 Grade 70

Yield strength is the stress at which the plate stops springing back and starts to stretch permanently. For Grade 70 the minimum is 260 MPa (38 ksi).

This is the number your design engineer works with most often, because a pressure vessel is not allowed to reach it in normal service. Note that the standard gives only a minimum. A plate testing at 320 MPa yield is perfectly acceptable, and most plates do test well above 260 MPa.

The gap between yield at 260 MPa and tensile at 485 MPa minimum is deliberately wide. That gap is your warning margin, because the vessel will visibly bulge and stretch long before it ruptures.

Elongation and Ductility

Elongation tells you how far the steel stretches before it snaps. It is measured by pulling a test piece to failure and recording how much longer it became, as a percentage.

A516 Grade 70 requires:

  • 17% minimum measured over a 200 mm (8 in.) gauge length, or
  • 21% minimum measured over a 50 mm (2 in.) gauge length

The two numbers describe the same steel. A short gauge length concentrates the stretching, so the percentage comes out higher. Your MTC will report whichever gauge length the mill used, and you do not need both.

Grade 70 has the lowest elongation requirement of the four A516 grades, because strength and ductility trade off against each other. Grade 55 must reach 23%, while Grade 70 only needs 17%.

Elongation Adjustments for Very Thin and Very Thick Plate

This is where most datasheets stop, and where real orders run into trouble.

ASTM A20, the umbrella standard that governs all pressure vessel plate, allows deductions from the minimum elongation at both ends of the thickness range:

  • Very thin plate. Below roughly 8 mm (0.312 in.), deductions of 0.5 to 5.0 percentage points apply as thickness drops.
  • Very thick plate. Above 89 mm (3.5 in.), deductions of 0.5 to 3.0 percentage points apply as thickness increases.

So a 5 mm plate and a 150 mm plate are both legitimately allowed to test below 17%, and the material still conforms. If you are inspecting an MTC and the elongation looks low, check the thickness before rejecting the heat.

Impact Toughness: The Property That is Not Included

A516 is designed for good notch toughness, but Charpy V-notch impact testing is not a standard requirement. It is a supplementary requirement that the purchaser must invoke on the purchase order. If you do not ask for it, the mill does not test for it, and your MTC will not report it.

If your vessel operates below about 0 °C, or your design code demands impact testing, you must specify:

  • The test temperature, for example −20 °C or −46 °C
  • The minimum absorbed energy, commonly 27 J average for process vessels
  • The specimen orientation, longitudinal or transverse

A typical process-industry requirement for Grade 70 is 27 J (20 ft·lbf) minimum at −46 °C on normalized plate. That performance is achievable, but only if it is ordered.

Hardness of A516 Grade 70

ASTM A516 does not specify a hardness value at all. Hardness is a useful indicator, not a pass or fail requirement.

Typical measured values are:

Condition Typical hardness
As-rolled 130–180 HB
Normalized 140–200 HB

Hardness does become a contractual requirement in sour service. Projects following NACE MR0175 or ISO 15156 often cap hardness at 200 HB or below to resist hydrogen-induced cracking. That cap must be written into the purchase order, because it is not part of A516.

How Plate Thickness Changes the Properties

The strength and elongation figures in the main table apply across the whole thickness range. What changes with thickness is the carbon content the mill is allowed to use and the delivery condition.

Plate thickness Maximum carbon (heat and product analysis)
Up to 12.5 mm (½ in.) 0.27%
Over 12.5 to 50 mm (½–2 in.) 0.28%
Over 50 to 100 mm (2–4 in.) 0.30%
Over 100 mm (4 in.) 0.31%

Thicker plate cools more slowly through the mill, so it needs a little more carbon to reach the same 485 MPa tensile minimum. The trade-off is weldability, because higher carbon means a higher carbon equivalent, which makes preheat more important during fabrication.

This matters commercially too. If you are ordering A516 Grade 70 plate cut to size rather than full mill plates, the parent plate thickness still governs which chemistry band and which delivery condition apply to your pieces. The cutting does not change the certification.

As-Rolled vs Normalized: A516 Gr 70 and Gr 70N

The same grade can be supplied in two different conditions, and the difference shows up in toughness rather than strength.

As-rolled vs normalized grain structure of A516 Gr 70 plate
Comparison Parameter  As-rolled (Gr 70) Normalized (Gr 70N)
Typical supply Plate up to 40 mm (1½ in.) Plate over 40 mm, mandatory
Grain structure Coarser, less uniform Refined and uniform
Low-temperature toughness Adequate Noticeably better
Hardness Slightly lower Slightly higher
Cost Lower Higher

The rule of thumb used across the industry is straightforward. Plates up to 40 mm are supplied as-rolled unless normalizing is specified, and plates over 40 mm are normalized as standard.

Normalizing means heating the plate to roughly 900–955 °C and cooling it in still air. It refines the grain structure and evens out the composition, which is what buys the improvement in low-temperature toughness.

If you need normalized plate below 40 mm, which is very common for cold-service vessels, you must write A516 Gr 70N or “normalized” on the purchase order. Ordering plain Grade 70 at 25 mm will get you as-rolled material.

One more condition is worth knowing. Simulated post-weld heat treatment, listed as Supplementary Requirement S3, applies when your vessel will be stress-relieved after welding. The plate spends hours at high temperature during that process, which slightly reduces its strength. S3 asks the mill to put the test coupons through the same thermal cycle first, so the certified properties reflect the plate as it will exist in the finished vessel rather than as it left the mill.

From Mechanical Properties to Design Values: Allowable Stress

A vessel is never designed to the tensile strength. It is designed to an allowable stress, a much lower figure with a safety margin built in.

Under ASME Section VIII Division 1, SA-516 Grade 70 has a maximum allowable stress of 20.0 ksi (138 MPa) at ambient temperature. That is the 70 ksi tensile minimum divided by a design margin of 3.5.

The value falls as temperature rises:

Metal temperature (°F) Allowable stress (ksi)
−20 to 500 20.0
600 19.4
650 18.8
700 18.1
750 14.8
800 12.0
850 9.3

One historical point matters when assessing older vessels. Before the 1999 addenda, ASME used a 4:1 design margin, so the allowable stress for SA-516 Gr 70 was 17.5 ksi rather than 20.0 ksi. If you are evaluating a vessel built before 1999, use the value from the code edition it was built to.

Note also that the plate holds a constant allowable stress up to roughly 500 °F before the numbers start dropping. Above about 850 °F, graphitization becomes a concern. A516 is a moderate-temperature steel, and it is not the right choice for sustained high-temperature service.

A516 Grade 70 vs Grades 55, 60 and 65

Grade Yield min (ksi) Tensile (ksi) Elongation in 8 in. (min)
55 30 55–75 23%
60 32 60–80 21%
65 35 65–85 19%
70 38 70–90 17%

The pattern is consistent. As you go up the grades you gain strength and lose ductility. Grade 70 lets you build a thinner, lighter vessel for the same pressure, while Grade 55 forms more easily and welds more forgivingly.

Grade 70 dominates the market for a practical reason as much as a technical one. It is the grade everyone stocks, so it is usually the fastest and cheapest to obtain regardless of what the calculation says. Where the calculation does put a lower grade within reach, the full comparison of A516 Grade 60, 65 and 70 sets out what you gain and lose at each step.

Equivalent Grades and How Their Properties Compare

Standard Equivalent grade Tensile strength Yield strength (min)
ASTM A516 Grade 70 485–620 MPa 260 MPa
ASME SA-516 Gr 70 485–620 MPa 260 MPa
EN 10028-2 P355GH 510–650 MPa 355 MPa (thin sections)
JIS G3115 SPV355 500–640 MPa 355 MPa
BS 1501 224-490 A/B 490–620 MPa ~355 MPa
IS 2002 Grade 3 (nearest) Comparable Comparable

Read this table carefully, because “equivalent” does not mean “identical.” P355GH is the closest European match and is frequently accepted as a substitute, but it carries a considerably higher minimum yield strength of 355 MPa against 260 MPa, along with a tighter carbon limit. It is normalized as standard and aimed at elevated-temperature service, whereas A516 Gr 70 is aimed at moderate and lower temperatures.

The practical consequence is that substituting P355GH for A516 Gr 70 is usually safe on strength, but the reverse substitution may not be. And if your vessel is ASME-coded, only SA-516 will satisfy the code. No European equivalent will do, however similar the numbers look.

How to Check the Mechanical Properties on Your MTC

Mill test certificate for A516 Grade 70 plate

When the Mill Test Certificate arrives, and EN 10204 Type 3.1 is the normal standard, work through it in this order:

  1. Heat number. Confirm it matches the marking stamped on the physical plate.
  2. Tensile result. Is it inside 485–620 MPa? Check both limits, not just the lower one.
  3. Yield result. Is it at or above 260 MPa?
  4. Elongation. Check which gauge length was used before comparing to 17% or 21%, and allow for A20 thickness deductions on very thin or very thick plate.
  5. Delivery condition. As-rolled, normalized, or normalized and stress relieved? Does it match what you ordered?
  6. Impact results. These appear only if you specified them. Check the test temperature and energy against your requirement.
  7. Dual certification. If you need SA-516, confirm the certificate explicitly names SA-516 and not only A516.

Common Mistakes When Specifying A516 Grade 70

  • Assuming impact testing is included. It is not. Specify it or you will not get it.
  • Ordering A516 when the vessel is ASME-coded. You need SA-516 on the paperwork.
  • Expecting normalized plate below 40 mm without asking. Write “Gr 70N” or “normalized.”
  • Treating tensile strength as a minimum only. The 620 MPa ceiling is a real rejection criterion.
  • Assuming a NACE hardness cap comes as standard. It does not. State it separately.
  • Using elevated-temperature allowable stress from the wrong code edition. Pre-1999 vessels use 17.5 ksi, not 20.0 ksi.
  • Treating P355GH as a drop-in replacement. It is similar, but not the same steel and not code-interchangeable.

Frequently Asked Questions

What is the tensile strength of A516 Grade 70?

The tensile strength is 485–620 MPa, or 70–90 ksi. Both limits apply, so a plate testing above 620 MPa is just as non-conforming as one testing below 485 MPa. Most mill-supplied plate lands in the 510–570 MPa range.

What is the yield strength of A516 Grade 70?

The minimum yield strength is 260 MPa, or 38 ksi. There is no upper limit, so plates commonly test well above this figure. Your design engineer works to the minimum, not the actual certified value.

What is the difference between A516 Gr 70 and Gr 70N?

The N stands for normalized, meaning the plate has been reheated to roughly 900–955 °C and cooled in still air. The strength requirements are identical for both. What changes is the grain structure, which becomes finer and more uniform in the normalized plate, giving noticeably better toughness at low temperatures.

Is A516 Grade 70 the same as SA516 Grade 70?

They are the same steel with the same requirements. A516 is the ASTM specification, while SA-516 is the version adopted into the ASME Boiler and Pressure Vessel Code. If your vessel is being built to the ASME code, your purchase order must say SA-516, and the mill certificate must name it explicitly.

What is the hardness of A516 Grade 70?

Typical hardness runs 130–180 HB in the as-rolled condition and 140–200 HB when normalized. ASTM A516 does not specify any hardness value, so these are indicative figures rather than requirements. If you need a hardness cap, most commonly 200 HB for sour service under NACE MR0175, you have to state it separately on the order.

What is the maximum operating temperature for A516 Grade 70?

Allowable stress stays constant at 20.0 ksi up to about 500 °F (260 °C), then falls steadily as temperature rises. The grade is intended for moderate and lower temperature service. Above roughly 850 °F (454 °C), graphitization becomes a genuine risk over long operating hours, so a different grade is usually the better choice for sustained high-temperature duty.

Does A516 Grade 70 need impact testing?

Only if you specify it. Charpy V-notch testing is a supplementary requirement rather than part of the base specification, so the mill will not perform it unless the purchase order asks. When you do specify it, state the test temperature, the minimum absorbed energy and the specimen orientation.

What is the minimum elongation of A516 Grade 70?

The requirement is 17% over a 200 mm gauge length or 21% over a 50 mm gauge length. The mill reports whichever gauge it used, and you only need one. ASTM A20 also permits deductions for very thin plate below about 8 mm and very thick plate above 89 mm, so a slightly lower result can still conform.

What is the equivalent of A516 Grade 70?

EN 10028-2 P355GH is the closest and most widely used equivalent. JIS G3115 SPV355 and BS 1501 224-490 are also comparable, and IS 2002 Grade 3 is the nearest Indian match. None of these can replace SA-516 on an ASME-coded vessel, so treat them as commercial alternatives rather than direct substitutes.

Is A516 Grade 70 easy to weld?

Yes, and good weldability is one of the main reasons the grade exists. Carbon equivalent can be capped at 0.43 (up to 25 mm) or 0.45 (over 25 mm) through Supplementary Requirement S54, and low-hydrogen consumables are recommended and moisture should be kept off the plate surface. Preheat becomes important above roughly 40 mm thickness, where the higher permitted carbon content raises the risk of cold cracking.

Conclusion

A516 Grade 70 gives you 485–620 MPa tensile strength, 260 MPa minimum yield, and 17% minimum elongation. That combination is chosen to be strong enough for real pressure vessels while staying ductile and weldable enough to fabricate safely.

The numbers themselves are simple. The judgement lies in what the standard leaves out. Impact toughness, hardness limits and the normalized condition below 40 mm are all optional, and every one of them has to be written onto the purchase order. Specify them properly and Grade 70 will do exactly what the design assumed. Leave them to chance and the certificate will still be valid, just not for the service you had in mind.

 

Need A516 Grade 70 plates with certified mechanical properties?

Send us your tensile, yield and impact requirements and we will confirm stock, sizes and mill test certificates.

Need A516 Grade 70 plates with certified mechanical properties?